  1. Hello, I am using mWare 1.1.9, and trying to print using white ABS. I have set the bed temperature to 110 degrees for every layer from -4 to +4. but the first couple of layers always print with a bed temperature of 80 degrees. Looking at the gcode file, the first instruction is M140 S80.000000, and the first layer is labelled -6. Is this intentional? Is there any way to get the first layers to print at 110 degrees for better raft adhesion? Is this actually a good idea? (I am new to ABS.)
×